塑胶原料报价
PPO PKN4752 高热量,FDA标准,食品级
  • 产 品:PPO PKN4752 高热量,FDA标准,食品级
  • 产 地:沙伯基础创新
  • 价 格:电话报价
  • 库 存:20吨
  • 交 货:江苏苏州
  • 苏州希普能:185 5121 3137 谭经理

Noryl* Food & Water Contact Resin
Food, Water, Medical Solutions
Modified amorphous blends of PPO* resin (polyphenylene ether) and polystyrenes.

Noryl* Resin PKN4752 英文物性表
PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and Healthcare Packaging.

Property
TYPICAL PROPERTIES(1)

MECHANICAL Value Unit  Standard 
Tensile Stress,yld,Type I,50mm/min 870 kgf/cm² ASTM D 638
Tensile Stress,brk,Type I,50mm/min 750 kgf/cm² ASTM D 638
Tensile Strain,yld,Type I,50mm/min 6 % ASTM D 638
Tensile Strain,brk,Type I,50mm/min 15 % ASTM D 638
Tensile Modulus,50mm/min 30600 kgf/cm² ASTM D 638
Flexural Stress,yld,1.3mm/min,50mm span 1470 kgf/cm² ASTM D 790
Flexural Stress,yld,2.6mm/min,100mm span 1390 kgf/cm² ASTM D 790
Flexural Modulus,1.3mm/min,50mm span 32100 kgf/cm² ASTM D 790
Flexural Modulus,2.6mm/min,100mm span 30000 kgf/cm² ASTM D 790
IMPACT Value Unit  Standard 
Izod Impact,notched,23℃ 3 cm-kgf/cm ASTM D 256
Instrumented Impact Total Energy,23℃ 66 cm-kgf ASTM D 3763
THERMAL Value Unit  Standard 
Vicat Softening Temp,Rate B/50 173 ASTM D 1525
HDT,0.45 MPa,3.2mm,unannealed 160 ASTM D 648
HDT,1.82 MPa,3.2mm,unannealed 151 ASTM D 648
HDT,1.82 MPa,6.4mm,unannealed 151 ASTM D 648
CTE,-40℃ to 40℃,flow 6.30E-05 1/℃ ASTM E 831
CTE,-40℃ to 40℃,xflow 5.58E-05 1/℃ ASTM E 831
PHYSICAL Value Unit  Standard 
Specific Gravity 1.08 - ASTM D 792
Mold Shrinkage,flow,3.2mm(5) 0.6-0.9 % SABIC Method
Source GMD,last updated:2002/08/16
Parameter Sheet Extrusion Value Unit 
Drying Temperature 70-80
Drying Time 2-4 hrs
Drying Time(Cumulative) 8 hrs
Maximum Moisture Content 0 %
Melt Temperature 265-275
Barrel-Zone 1 Temperature 205-225
Barrel-Zone 2 Temperature 215-240
Barrel-Zone 3 Temperature 240-265
Barrel-Zone 4 Temperature 240-265
Adapter Temperature 240-265
Die Temperature 240-265
Roll Stack Temp-Top 105-120
Roll Stack Temp-Middle 105-120
Roll Stack Temp-Bottom 105-120
Source GMD,last updated:2002/08/16

• Use lower process temperatures when material is let-down.

THESE PROPERTY VALUES ARE NOT INTENDED FOR SPECIFICATION PURPOSES.
Buy SABIC Innovative please contact xiang zhang Engineering plastics
1、Typical values only. Variations within normal tolerances are possible for various colors. All values are measured after at least 48 hours storage at 23℃/50% relative humidity. All properties, except the melt volume and melt flow rates, are measured on injection molded samples. All samples tested under ISO test standards are prepared according to ISO 294.
2、Only typical data for selection purposes. Not to be used for part or tool design.
3、This rating is not intended to reflect hazards presented by this or any other material under actual fire conditions.
4、Internal measurements according to UL standards.
5、Measurements made from laboratory test coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.